0. Dryer Length in M. 11.25. 7.5. 3.75. Dryer Type "S". Typical Drying Profile for 80 gsm UF/MF Product @ 45m/min. T = 140 °C. T = 160 °C. T = 170 °C. V = 22 m/s. V = 18 m/s. V = 15 m/s. Typically 3 Sections á 3.75 m. Zone Temperature Range100 to 220 °C.
E N D
0 Dryer Length in M 11.25 7.5 3.75 Dryer Type "S" Typical Drying Profile for 80 gsm UF/MF Product @ 45m/min T = 140 °C T = 160 °C T = 170 °C V = 22 m/s V = 18 m/s V = 15 m/s • Typically 3 Sections á 3.75 m • Zone Temperature Range100 to 220 °C • Air Speed at Nozzle 12 to 22 m/s
°C % 60 120 50 100 40 80 30 60 20 40 10 20 T = 170 °C T = 160 °C T = 140 °C V = 18 m/s V = 15 m/s V = 22 m/s 0 Dryer Length in M 11.25 7.5 3.75 Dryer Type "S" Typical Drying Profile for 80 gsm UF/MF Product @ 45m/min Web Temperature 110 - 120°C Moisture Content 12 - 14% • Exit Moisture (Volatiles) 10 to 16 % • Web Temperature Rise 20 to 120 °C
Dryer I Type "S" • Avoids • Edge Flatter • Paper Wrinkles • Surface Defects • Gives • Contactless Drying • Uniform Moisture Content • Variable heat transfer • Fast Start Up
Mini Cooling Section Meyerbar & Smoothing Roll Stand Gravure Rolls Intermediate Section
Mini Cooling Zone • Floatation Nozzles • Lowers Web Temperatureprior to coating • Supports Web for 1 StageOperation
Gravure Roll Coater • For Two Stage OperationLP Decorative Papers • Fixed MF Coating WeightIrrespective of raw paper coating • Independent to web tension • Gravure Rolls with defined “Nip” Size • Thousands of “Nips” over width of roll • Wet Coating 20 to 30 gsm on each Side varied by roll speed to paper
Meyerbar & Smoothing Rolls • 2 Meyerbar rolls spread out coating ”Tyre Print” caused by gravure roll “Nips” over web width • 2 Smoothing Rolls Polish Product Surface Prior to Dryer II • Unit can be moved apart for cleaning & Gravure roll exchange
Dryer II Type "S" • Drives out moisture from core resin • Carries on the UF/MF core resin part curing • Drives out moisture from MF Surface Resin coating • Starts MF Resin part curing • Reduces moisture (volatiles) down to required final volatile content:5.8 to 6.5 % • Same dryer design as for stage I
0 22.5 15.0 11.25 3.75 7.5 18.75 Dryer Length in M Dryer II Type "S" Typical Drying Profile for 80 gsm UF/MF Product @ 45m/min T = 140 °C T = 150 °C T = 160 °C T = 150 °C T = 140 °C T = 130 °C V = 15 m/s V = 15 m/s V = 15 m/s V = 18 m/s V = 18 m/s V = 18 m/s • Zone Temperature Range100 to 220 °C • Air Speed at Nozzle 12 to 22 m/s • Typically 6 Sections á 3.75 m
°C % 60 120 50 100 40 80 30 60 20 40 10 20 T = 140 °C T = 150 °C T = 160 °C T = 150 °C T = 140 °C T = 130 °C V = 15 m/s V = 15 m/s V = 15 m/s V = 18 m/s V = 18 m/s V = 18 m/s 0 22.5 15.0 11.25 7.5 18.75 3.75 Dryer Length in M Dryer II Type "S" Typical Drying Profile for 80 gsm UF/MF Product @ 45m/min Web Temperature 110 - 120°C Moisture Content 5.8 - 6.5% • Exit Moisture (Volatiles) 5.8 to 6.5% • Web Temperature Rise 20 to 120 °C
Dryer II Type "S" • Too Aggressive Drying • Damage Surfacepin holescracks • Increased melamine Dusting • High Static Electricitycharging • High Formaldehyde emissions