An Image/Link below is provided (as is) to download presentation Download Policy: Content on the Website is provided to you AS IS for your information and personal use and may not be sold / licensed / shared on other websites without getting consent from its author. Content is provided to you AS IS for your information and personal use only. Download presentation by click this link. While downloading, if for some reason you are not able to download a presentation, the publisher may have deleted the file from their server. During download, if you can't get a presentation, the file might be deleted by the publisher.

E N D

Presentation Transcript


  1. OUTLINE Poisson’s Equation Work function Metal-Semiconductor Contacts equilibrium energy-band diagram depletion-layer width Read: Chapter 5.1.2,14.1, 14.2 Lecture #10 EE130 Lecture 10, Slide 1

  2. Poisson’s Equation Gauss’s Law: area A s :permittivity (F/cm)  :charge density (C/cm3) E(x) E(x+Dx) Dx EE130 Lecture 10, Slide 2

  3. Charge Density in a Semiconductor • Assuming the dopants are completely ionized: r = q (p – n + ND – NA) EE130 Lecture 10, Slide 3

  4. Work Function E0: vacuum energy level FM: metal work function FS: semiconductor work function EE130 Lecture 10, Slide 4

  5. Metal-Semiconductor Contacts There are 2 kinds of metal-semiconductor contacts: • rectifying “Schottky diode” • non-rectifying “ohmic contact” EE130 Lecture 10, Slide 5

  6. Ideal MS Contact: FM >FS, n-type Band diagram instantly after contact formation: Schottky Barrier : Equilibrium band diagram: EE130 Lecture 10, Slide 6

  7. Ideal MS Contact: FM <FS, n-type Band diagram instantly after contact formation: Equilibrium band diagram: EE130 Lecture 10, Slide 7

  8. Ideal MS Contact: FM <FS, p-type metal p-type Si Eo cSi Ec FM EF Ev FBp = c + EG -FM FBp qVbi = FBp– (EF – Ev)FB W EE130 Lecture 10, Slide 8

  9. Effect of Interface States on FBn FM >FS metal n-type Si • Ideal MS contact: FBn=FM– c • Real MS contacts: • A high density of allowed energy states in the band gap at the MS interface pins EF to the range 0.4 eV to 0.9 eV below Ec Eo cSi FM qVbi = FB – (Ec – EF)FB FBn Ec EF Ev W EE130 Lecture 10, Slide 9

  10. Schottky Barrier Heights: Metal on Si • FBn tends to increase with increasing metal work function EE130 Lecture 10, Slide 10

  11. Schottky Barrier Heights: Silicide on Si Silicide-Si interfaces are more stable than metal-silicon interfaces. After metal is deposited on Si, a thermal annealing step is applied to form a silicide-Si contact. The term metal-silicon contact includes silicide-Si contacts. EE130 Lecture 10, Slide 11

  12. The Depletion Approximation • The semiconductor is depleted of mobile carriers to a depth W • In the depleted region (0  x  W ): r = q (ND – NA) Beyond the depleted region (x > W ): r = 0 EE130 Lecture 10, Slide 12

  13. Electrostatics E • Poisson’s equation: • The solution is: E E EE130 Lecture 10, Slide 13

  14. Depleted Layer Width, W At x = 0, V = -Vbi • W decreases with increasing ND EE130 Lecture 10, Slide 14

  15. Summary: Schottky Diode (n-type Si) FM >FS metal n-type Si Equilibrium (VA = 0) -> EF continuous, constant • FBn =FM – c Depletion width: Eo cSi FM qVbi = FBn – (Ec – EF)FB FBn Ec EF Ev W EE130 Lecture 10, Slide 15

  16. Summary: Schottky Diode (p-type Si) FM <FS metal p-type Si Eo Depletion width: cSi Ec FM Equilibrium (VA = 0) -> EF continuous, constant FBp = c + EG -FM EF Ev FBp qVbi = FBp– (EF – Ev)FB W EE130 Lecture 10, Slide 16