Cyanidlaugerei. Zerkleinertes Gestein. Durchlüftung. KCN (oder NaCN - Lösung). 4 Au + 8 KCN + 2 H 2 O + O 2 → 4 K[Au(CN) 2 ] + 4 KOH. Zn Staub. Reduktion. 2 K[Au(CN) 2 ] + Zn → K 2 [ Zn (CN) 4 ] + 2 Au. Schlamm mit Au und Zn. Filtration. Au. Amalgamverfahren.

harken
Download Presentation

Cyanidlaugerei

An Image/Link below is provided (as is) to download presentation Download Policy: Content on the Website is provided to you AS IS for your information and personal use and may not be sold / licensed / shared on other websites without getting consent from its author. Content is provided to you AS IS for your information and personal use only. Download presentation by click this link. While downloading, if for some reason you are not able to download a presentation, the publisher may have deleted the file from their server. During download, if you can't get a presentation, the file might be deleted by the publisher.

E N D

Presentation Transcript


  1. Cyanidlaugerei Zerkleinertes Gestein Durchlüftung KCN (oder NaCN- Lösung) 4 Au + 8 KCN + 2 H2O + O2→4 K[Au(CN)2] + 4 KOH Zn Staub Reduktion 2 K[Au(CN)2] + Zn → K2[Zn(CN)4] + 2 Au Schlamm mit Au und Zn Filtration Au

  2. Amalgamverfahren Zerkleinertes und goldhaltiges Gestein Wasser Hg Pochtrübe AuHgx AuHgx Kondensation Au Destillation

More Related