Stages of the patch repair; Hand-applied mortar

Stages of the patch repair; Hand-applied mortar. Rak-43.3312 Repair Methods of Structures II (4 cr) Esko Sistonen. 1. Locate damaged areas. Fig . J. Mattila. 2. Removing damaged concrete. Fig . J. Mattila. 3a. Cleaning surfaces. Fig . J. Mattila. 3b. Wetting surfaces.

hesper
Download Presentation

Stages of the patch repair; Hand-applied mortar

An Image/Link below is provided (as is) to download presentation Download Policy: Content on the Website is provided to you AS IS for your information and personal use and may not be sold / licensed / shared on other websites without getting consent from its author. Content is provided to you AS IS for your information and personal use only. Download presentation by click this link. While downloading, if for some reason you are not able to download a presentation, the publisher may have deleted the file from their server. During download, if you can't get a presentation, the file might be deleted by the publisher.

E N D

Presentation Transcript


  1. Stages of the patch repair; Hand-applied mortar Rak-43.3312 Repair Methods of Structures II (4 cr) Esko Sistonen

  2. 1. Locate damaged areas Fig. J. Mattila

  3. 2. Removing damaged concrete Fig. J. Mattila

  4. 3a. Cleaning surfaces Fig. J. Mattila

  5. 3b. Wetting surfaces Ref. Betonijulkisivujen korjaus laastipaikkauksella, Rakennustieto 1995

  6. 4 & 5. Spreading corrosion preventing agent and primer Fig. J. Mattila

  7. 6 & 7. Spreading patch and finishing mortar Fig. J. Mattila

  8. 8. After-treatment Fig. J. Mattila

  9. 9. Coating