A luminum Stud Welding Technologies. By Chris Hsu and Clark Champney Nelson Stud Welding, Inc. . Challenges. Low melting point High thermal conductivity Tough oxide (3488F) Spatter Softening. Drawn Arc Stud Welding 101. A. Pilot Arc. B. Lift Main Arc. C. Plunge. D. Remove
E N D
Aluminum Stud Welding Technologies By Chris Hsu and Clark Champney Nelson Stud Welding, Inc. 2011 AWS Conference and Exhibition Welding in Shipbuilding
Challenges • Low melting point • High thermal conductivity • Tough oxide (3488F) • Spatter • Softening
Drawn Arc Stud Welding 101 A. Pilot Arc B. Lift Main Arc C. Plunge D. Remove Chuck
Capacitor discharge AWS Seattle May 10, 2011
CD welding Process • Weld time • Timing tip • Plunge speed • Current • Cap voltage • Cable impedance • Contact • Gap • Stored Arc 2011 AWS Conference and Exhibition Welding in Shipbuilding
MIL specifications • MIL-S-24149/2D: aluminum stud and ferrule for drawn arc • MIL-S-24149/5C: aluminum stud for CD and stored arc AWS Seattle May 10, 2011
Gun accessories • Gas foot • Tranquil arc plunge dampener • Motorize gun AWS Seattle May 10, 2011
plate thickness to stud diameter ratio • Develop full strength • Steel: 1/3 • Aluminum (Al is annealed in stud welding) • ½ for drawn arc • ¼ for CD AWS Seattle May 10, 2011
Weld strength: tensile/torque AWS Seattle May 10, 2011
Internally threaded studs • Diameter ¼” to ½” • Threads #10-24 thru ½-13 • 5000 series alloy used for stud (Magnesium based) • LNG tankers AWS Seattle May 10, 2011
Pulse cleaning and welding • Cut oxide, rust, oil, mill-scale • Reduce heat input • backside marking • Stiffen arc • Out of position • Angle iron • Aluminum • Peak: cathodic clean • Background: heat Stud Welding Technologies – ShipTech 2011
Process monitor & loggerWelder, Gun and Cable • Weld energy • Stud hang-up • Cold plunge • Cable overheat • Weld Pass / Fail • Production log Normal Cold Stud Welding Technologies – ShipTech 2011 Hang-up Hot
Summary • CD - contact, gap and stored arc • Drawn arc • Pulse • AC • Up to ½” can be welded down hand and plate vertical • Inverter to weld 5/8” and ¾” in flat position • Process monitor • Drawn arc • CD 2011 AWS Conference and Exhibition Welding in Shipbuilding