Cu of Norddeutsche Affinerie (Hamburg, Germany) melting casting cathodes anodes NOSV quality 99.9975% (1-4 ppm O2) 97-99 % + 2000 ppm O2 +... Ni: % IN ORE < !-2 ppm Co: about 5 ppm < 1 ppm 40K: 7.5 1.0 mBq/kg < 0.088 mBq/kg 226Ra: 1.8 0.4 mBq/kg < 0.020 mBq/kg 228Th: < 0.44 mBq/kg < 0.023 mBq/kg under investigation E.Pernicka
Norddeutsche Affinerie is very open to our needs take special care in the cathode production and provide the cast material a few days after the removal from the electrolyses for further processing without forming = 8.7 g/cm3 after hot forming: 8.92 g/cm3 full of small porous mainly containing H2 Acid cleaning difficult (sticks in pores) electropolishing o.k. smoothes the surface possible electrodeposition or selfdepostion of 210Po is investigated by M. Wojcik
+ 270 d 125 kg NOSV Cu for LENS measured with GeMPI M. Laubenstein G. Heusser preliminary +