1 / 4

D1655 vs. D 7566 Specification Overview

D1655 vs. D 7566 Specification Overview. Joseph Sorena 11/3/2011. D7566 Structure. Synthetic Paraffinic Kerosene (SPK) blend components. FT SPK Table A1.1 Lower total acid T90-10 Min Thermal Stability Limit Temperature Elevated to 325 C. Anti-Oxidant Required (17 min 24 mg/L max)

rod
Download Presentation

D1655 vs. D 7566 Specification Overview

An Image/Link below is provided (as is) to download presentation Download Policy: Content on the Website is provided to you AS IS for your information and personal use and may not be sold / licensed / shared on other websites without getting consent from its author. Content is provided to you AS IS for your information and personal use only. Download presentation by click this link. While downloading, if for some reason you are not able to download a presentation, the publisher may have deleted the file from their server. During download, if you can't get a presentation, the file might be deleted by the publisher.

E N D

Presentation Transcript


  1. D1655 vs. D 7566 Specification Overview Joseph Sorena 11/3/2011

  2. D7566 Structure

  3. Synthetic Paraffinic Kerosene (SPK) blend components • FT SPK Table A1.1 • Lower total acid • T90-10 Min • Thermal Stability Limit Temperature Elevated to 325 C. • Anti-Oxidant Required (17 min 24 mg/L max) • Cycloparaffin 15 Mass % Max • Aromatics 0.5 Mass % Max • Carbon & Hydrogen 99.5% Min • Nitrogen 2 ppm Max • Water 75 ppm Max • Sulfur 15 ppm Max • Metals 0.1 ppm Max • Halogens 1 ppm Max • HEFA Table A2.1 • All requirements as A1.1 plus • Fame less than 5 ppm

  4. Other considerations D7566 • 50 vol % blend max of SPK with Conventional Jet • With respect to ASTM the fuel will be distributed and handled as 1655 once blended and released. • Additives are the same approved for D1655 • Synthetic Aromatics Feedstocks outside of Scope of D7566 • Alcohol to Jet • Pyrolysis oils