Thermal cycle and Hardness. 780ºC 2h + 820 º C 6min. 1mm. Cell 1, before and after heating. Before. After. 1mm. Cell 3, before and after heating. Before. After. After heating. Detail of general aspect. After heating. Details of stains and spots.
E N D
Thermal cycle and Hardness. 780ºC 2h + 820ºC 6min CLIC not used cells - SM Group
1mm Cell 1, before and after heating. Before After CLIC not used cells - SM Group
1mm Cell 3, before and after heating. Before After CLIC not used cells - SM Group
After heating. Detail of general aspect CLIC not used cells - SM Group
After heating. Details of stains and spots. CLIC not used cells - SM Group
After heating. Details of stains and spots. CLIC not used cells - SM Group
Grain size. Before (Cell 2) After CLIC not used cells - SM Group
Facetting. CLIC not used cells - SM Group
Lathe work mismatch. Slight mismatch in Cell 2 20µm mismatch in Cell 3 CLIC not used cells - SM Group