Overview of ACCC Composite Core - CTC Global

CTC Global manufactures ACCC Composite Core that has strength to weight ratio approximately six times better than steel, with coefficient of thermal expansion ten times lower.<br>Contact Us:<br>Phone: 1 949 428 8500<br>info@ctcglobal.com<br>www.ctcglobal.com<br>

ctcglobal
Download Presentation

Overview of ACCC Composite Core - CTC Global

An Image/Link below is provided (as is) to download presentation Download Policy: Content on the Website is provided to you AS IS for your information and personal use and may not be sold / licensed / shared on other websites without getting consent from its author. Content is provided to you AS IS for your information and personal use only. Download presentation by click this link. While downloading, if for some reason you are not able to download a presentation, the publisher may have deleted the file from their server. During download, if you can't get a presentation, the file might be deleted by the publisher.

E N D

Presentation Transcript


  1. Overview of ACCC Composite Core- CTC Global www.ctcglobal.com Aug 2019

  2. About CTC Global CTC Global was founded to improve the efficiency, capability, reliability and resiliency of the electric power grid. CTC global began development of high capacity, low sag ACCC conductors in early 2003. In addition to producing the CTC Global ACCC conductor’s hybrid carbon and glass fiber ACCC core, CTC Global also produces a number of components used in various connectors such as dead-ends and splices. The ACCC conductor’s hybrid composite core produced by CTC Global reduces thermal sag that limits the current carrying capacity of other conductor types. www.ctcglobal.com

  3. Learn about ACCC Composite Core The ACCC Composite Core conductor is made up of high carbon and glass fibersembedded in a toughened thermoset epoxy resin matrix. The composite core is manufactured using a continuous pultrusion process by highly skilled pultrusion experts. www.ctcglobal.com

  4. Offerings by ACCC Composite Core • The ACCC Composite Core offers a strength to weight ratio approximately six times better than steel. • Coefficient of thermal expansion about ten times lower.  • It is impervious to corrosion and cyclic load fatigue. www.ctcglobal.com

  5. The availability ACCC Composite Core are currently available in • 310 ksi tensile strength • 375 ksi tensile strength • Higher strength version - ULS www.ctcglobal.com

  6. ULS offerings ULS id basically the higher strength version of ACCC Composite core. It offers higher modulus to accommodate longer spans and extreme ice loads. www.ctcglobal.com