1 / 5

300ºC Tin isopropoxide 2011.2.25

Experiment. ZnSnO x (ZTO) Sn Precursor - SnCl 4. 300ºC Tin isopropoxide 2011.2.25. 300ºC Tin(IV) chloride 2011.3.1. Experiment. Low mobility yet ~0.003. Sample 1. Sample 2. Experiment. Poor bias stress stability. Sample 3, 1 st measure. Sample 3, 2 nd measure. Experiment.

devlin
Download Presentation

300ºC Tin isopropoxide 2011.2.25

An Image/Link below is provided (as is) to download presentation Download Policy: Content on the Website is provided to you AS IS for your information and personal use and may not be sold / licensed / shared on other websites without getting consent from its author. Content is provided to you AS IS for your information and personal use only. Download presentation by click this link. While downloading, if for some reason you are not able to download a presentation, the publisher may have deleted the file from their server. During download, if you can't get a presentation, the file might be deleted by the publisher.

E N D

Presentation Transcript


  1. Experiment ZnSnOx (ZTO) SnPrecursor-SnCl4 300ºC Tin isopropoxide 2011.2.25 300ºC Tin(IV) chloride 2011.3.1

  2. Experiment Low mobility yet ~0.003 Sample 1 Sample 2

  3. Experiment Poor bias stress stability Sample 3, 1st measure Sample 3, 2nd measure

  4. Experiment No UV irradiation effect Sample 3 (UV treated)

  5. Future work • Mobility 0.026cm2/vs • Solution optimization • Acetic acid catalyst • Bias stress hysteresis – origin analysis