Shear Tests - DIPTEM Genova. A dhesive tape NITTO DENKO 30 µm thick. Adhesive tape 3M 9461P – 30 µm thick. Liquid glue Araldite 2020. Adhesive film FastelFilm 30 µm thick. Silicon. Polyester film double coated by acrylic adhesive Polyester = 0.13-0.15 W/m K Acrilyc = 0.2 W/m K.
E N D
Shear Tests - DIPTEM Genova Adhesive tape NITTO DENKO 30 µm thick Adhesive tape 3M 9461P – 30 µm thick Liquid glue Araldite 2020 Adhesive film FastelFilm 30 µm thick Silicon • Polyester film double coated by acrylic adhesive • Polyester = 0.13-0.15 W/m K • Acrilyc = 0.2 W/m K • 3M Adhesive 100 (Acrylic adhesive) • 3M Adhesive 100 = 0.178 W/m K • Two components epoxy liquid glue • Epoxy = 0.188 W/m K • EVA (Ethylene - vinyl Acetate) adhesive film • EVA = 0.34 W/m K • Surface cleaning with acetone • 1 Kg for 65 hours • Surface cleaning with acetone • 1 Kg for 65 hours • Surface cleaning with acetone • Vacuum outgassing after mixing the component • Dispensing with a blade • Surface cleaning with acetone • 1 Kg for 3 minutes • 80 °C in the oven (weight and plate already hot) Silicon glue Silicon samples 10 x 10 mm Araldite: 2 samples FastelFilm: 4 (2 with the weight 2 without) NittoDenko: 4 (2 with the weight 2 without) 3M: 4 (2 with the weight 2 without)
Shear Tests - DIPTEM Genova - Machine INSTRON 8802 – Floor Model Fatigue Testing Systems Top clamp Bottom clamp Working set up
Gluing Tests - DIPTEM Genova - Results S1 and S2 = withoutweight of 1 kg on top S1 and S2 = withoutweight of 1 kg on top
Gluing Tests - DIPTEM Genova - Results S1 and S2 = withoutweight of 1 kg on top