930 likes | 2.48k Views
Tensile Testing. Classic Necking Behavior of Tensile Specimen. P&WA Automated Tensile Test Apparatus. P&WA High Temperature Air Cooled Extensometer. Fractured Tensile Specimen/Test Temperature 2000 °F. True Stress and Strain. Al alloy. Ni alloy. Ti alloy.
E N D
Al alloy Ni alloy Ti alloy
PWA 1480 single crystal Yield Strength as a function of temperature and orientation <001> <011> <111> <111>
[001] [111] [001] [111] PWA1480 SC tensile fracture versus crystal orientation
PWA 1480 single crystal Tensile Elongation as a function of temperature and crystal orientation Crystallographic shear failure Tensile Elongation, % Temperature, °C, (°F)
(111) (001) (011) PWA 1480 single crystal Elastic Modulus at RT as a function of orientation Elastic Behavior <111> 42 msi <100> 18 msi <110> 30 msi
PWA 1480 Yield Strength - Crystal Orientation dependence: Tension/Compression asymmetry T = tensile YS C = compressive YS