SVA Whisker Testing / Results

SVA Whisker Testing / Results. As a whisker mitigation measure, National anneals all of its tin plated, leadframe-based packages for 1 hour at 150° C within 24 hours of plating. This is the industry-accepted method for controlling whisker growth.

wanda
Download Presentation

SVA Whisker Testing / Results

An Image/Link below is provided (as is) to download presentation Download Policy: Content on the Website is provided to you AS IS for your information and personal use and may not be sold / licensed / shared on other websites without getting consent from its author. Content is provided to you AS IS for your information and personal use only. Download presentation by click this link. While downloading, if for some reason you are not able to download a presentation, the publisher may have deleted the file from their server. During download, if you can't get a presentation, the file might be deleted by the publisher.

E N D

Presentation Transcript


  1. SVA Whisker Testing / Results • As a whisker mitigation measure, National anneals all of its tin plated, leadframe-based packages for 1 hour at 150° C within 24 hours of plating. This is the industry-accepted method for controlling whisker growth. • Since thin plating is known to be more susceptible to whisker growth, National maintains a minimum tin plating thickness of 8 microns, with a nominal thickness of 12 microns. • National packages are plated with the most advanced plating chemistry in the industry for tin whisker control and have been meeting JEDEC 22A121 specifications since 2010. • In terms of lead-free requirements, the current RoHS Directive exempts leadframe packages with pitches less than or equal to 0.65 mm. • The following data is collected per the JEDEC requirements given in JESD201

  2. SVA Whisker Testing / Results

More Related