Transmission-Type Pump-Probe ZnO/ ZnMgO MQW 365 to 385 nm Measured@20091026. 1. Construction 2. Absorption Spectrum 3. PL Spectrum. Optical Properties. ZnMgO MQW. PL (55K). Substrate (c-Al 2 O 3 ). MZO (15 min, ~21nm). ZnO (5 min, ~7nm 可能更小 ). 5 pair MgZnO/ZnO.
E N D
Transmission-Type Pump-Probe ZnO/ZnMgO MQW 365 to 385 nm Measured@20091026
1. Construction 2. Absorption Spectrum 3. PL Spectrum Optical Properties
ZnMgO MQW PL (55K) Substrate (c-Al2O3) MZO (15 min, ~21nm) ZnO (5 min, ~7nm 可能更小) 5 pair MgZnO/ZnO MgxZn1-xO, x=0.05
Comparison of Exciton Dynamics1. ZnO thin film (70nm)2.MgZnO SQW3. MgZnO MQW
Absorption Spectrum
ZnO (70nm)@ 372.5nm Pr=0.5, PP=20mW 0.9ps 8.5ps 50ps
ZnMgO SQW (1pair) Pr=0.5, PP=20mW y=y0+A1exp(t1)+A2exp(t2)+A3exp(t3)
375nm [Pr=1mW PP=20mW] y=y0+A1exp(t1)+A2exp(t2)+A3exp(t3)
ZnMgO MQW (5pairs) Pr=0.5, PP=20mW y=y0+A1exp(t1)+A2exp(t2) Substrate (c-Al2O3)
Energy dependent Dynamics in MgZnO MQW1. above-band-gap2.near-band-gap3. below-band-gap
y=y0+A1exp(t1)-A2exp(t2) 363 nm [Pr=0.5mW PP=10mW] y=y0+A1exp(t1)+A2exp(t2) 365 nm [Pr=0.5mW PP=10mW]
368 nm [Pr=0.5mW PP=10mW] T0= 63 mV y=y0+A1exp(t1)+A2exp(t2)
370nm [Pr=0.5mW PP=10mW] T0= 50 mV y=y0+A1exp(t1)+A2exp(t2)
373nm [Pr=0.5mW PP=10mW] T0= 36 mV y=y0+A1exp(t1)+A2exp(t2)
375nm [Pr=0.5mW PP=10mW] y=y0-A1exp(t1)-A2exp(t2)
377nm [Pr=0.5mW PP=10mW] T0= 320 mV y=y0-A1exp(t1)-A2exp(t2)
379nm [Pr=0.5mW PP=10mW] T0= 810 mV y=y0-A1exp(t1)
385nm [Pr=0.5mW PP=10mW] T0= 860 mV y=y0+A1exp(t1)