Utilisation of the -8+5mm Sishen iron ore fraction in the Sintering process September 2008 Andre Dippenaar

Utilisation of the -8+5mm Sishen iron ore fraction in the Sintering process September 2008 Andre Dippenaar. Sishen mine products : Lump ore: -25+8mm Fine ore: -5mm Intermediate fraction: -8+5mm. Introduction. Pilot Plant Sinter Pot tests Bc sinter – 50% fine Thaba, 50% fine Sishen

twyla
Download Presentation

Utilisation of the -8+5mm Sishen iron ore fraction in the Sintering process September 2008 Andre Dippenaar

An Image/Link below is provided (as is) to download presentation Download Policy: Content on the Website is provided to you AS IS for your information and personal use and may not be sold / licensed / shared on other websites without getting consent from its author. Content is provided to you AS IS for your information and personal use only. Download presentation by click this link. While downloading, if for some reason you are not able to download a presentation, the publisher may have deleted the file from their server. During download, if you can't get a presentation, the file might be deleted by the publisher.

E N D

Presentation Transcript


  1. Utilisation of the -8+5mm Sishen iron ore fraction in the Sintering processSeptember 2008Andre Dippenaar

  2. Sishen mine products: Lump ore: -25+8mm Fine ore: -5mm Intermediate fraction: -8+5mm Introduction

  3. Pilot Plant Sinter Pot tests Bc sinter – 50% fine Thaba, 50% fine Sishen Coarse Sinter - Half of fine Sishen replaced with coarse Sishen50% fine Thaba, 25% fine Sishen, 25% coarse Sishen Concentrate additions – 5, 10 and 15 %

  4. Sinter spesifications % SiO2 5.2 % MgO 0.77 % FeO 8.0 Basicity %CaO/SiO2 = 2.0 Experimental Procedure

  5. Sinter working procedures Sinter outputs Tests on sinter product Experimental Procedure

  6. Results – Ore fractions used Ore Sieve analyses

  7. Identification of the different pot tests: Fine Sishen sinters FS 0C - Base case sinter with 50% Fine Sishen and 0% Concentrate FS 5C - Fine sinter with 45% Fine Sishen and 5% Conc. Coarse Sishen sinters CS 0C - Coarse sinter with 25%Fine Sishen, 25% Coarse Sishenand 0% Conc. CS 5C - Coarse sinter with 20%Fine Sishen, 25% Coarse Sishenand 5% Conc CS 10C - Coarse sinter with 15% Fine Sishen, 25% Coarse Sishenand 10% Conc. CS 15C - Coarse sinter with 10%Fine Sishen, 25% Coarse Sishenand 15% Conc Results

  8. Results Raw material Mixture Sieve analyses • FS 0C – 2.5 mm • CS 0C – 3.23 mm

  9. Results - Sinter Pot Tests

  10. Results – Production Rate

  11. Results – Fuel Consumption

  12. Results – Cake Shrinkage

  13. Results – Sinter Product size

  14. Results – Physical and Metallurgical properties

  15. Results – Cold Strength

  16. Results – Hot strength +3.15 mm

  17. Results – Hot strength -0.5mm

  18. Results – Reducibility

  19. Results – High temperature properties

  20. Results – High temperature properties

  21. Results – Mineralogy

  22. Results – Mineralogy

  23. Results – Mineralogy